The Development of Advanced Nickel-Based Superalloys

The Development of Advanced Nickel-Based Superalloys

Nickel-base superalloys consist of austenitic matrix structures enriched with elements like cobalt, iron, molybdenum and aluminum that act as solid-solution strengtheners. When these are heated-treated, precipitation of an FCC phase known as g' is promoted - increasing in strength wi